· About % of the aluminium was leached from the washed residue by pressure leaching at 240 °C, using 260 g/L NaOH. The resulting leach liquor contained mainly aluminium which could be recovered by crystallization, in the form gibbsite (Bayer process). Experimental Aluminium black dross characterization